I've done some 4% melts in the past when I was using a ceramics kiln and using spectrum cullet as my base. It was far from even an okay setup but I did run into issues of having some kind of precipitate or haze at the bottom of my crucibles. For compatibility, you'll be straddling the line between compatible and not though most cases it'll be not.
Again, this setup was pretty bad but I figured I'd give my two cents.