Use the search engine on this site, I have written lots of stuff in the past that details all of this stuff. As to suppliers, I am importing moly's, Or I squared R makes them domestically or Kanthal corp.

Check the archives.

P.S. my favorite supplier of electrical components is Watlow. Excellent customer support and technical assistance.