what came out of the annealer today
So the white pieces that were cased looked real nice. I made a pineapple mold ball from just the white and it feels like sandpaper on the surface.
Perhaps I did not melt hot enough, and I probably put too much in at one time. These are things that now I know I can fix I also will have to balance which colors and how I charge with regard to doing the hotter ones first.
Thank you John Croucher and to everyone that chimed in on this project. I will go back and study some more, hopefully to make this better next time.
__________________
Rich
|