Quote:
Originally Posted by Pete VanderLaan View Post
Gold glasses can liver in reflective light if the molecules get big enough and I suspect that's what you are seeing. I make a gold chloride solution for my rubies and then mix it in gold sands. My friend john just pours the gold chloride into the batch,
There are three important things in the receiving batch, Gold , lead and selenium.
By livering, do you mean a colloidal solution is formed in the glass of gold and possibly silver nanoparticles/nanospheres? What do the lead and selenium have to do with the gold?