View Single Post
  #27  
Old 07-10-2018, 01:51 PM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 23,870
Pete VanderLaan is on a distinguished road
Use a decent scale and mixer. Care is a handy commodity. You can be as open with the supply houses as you choose to be. Cristalica is entering the supply phase I referred to a few months back. Watch how that plays out in terms of QC. I just keep mixing my own or I have SP mix it for me in tonnage.
__________________
Where are we going and why am I in this basket?