I just looked at US Pigment again and the only one I had seen in the past was their 325 mesh/99.9@ NdO for $60/lb. But I do now see they offer that $25/lb. option for 95.5% but it's called "coarse". I haven't bought any from them, I'm towards the end of the stuff I bought from Dudley, but I'm guessing that was closer to a 325 mesh. Now I'm wondering if the coarser mesh will work just fine. The concentration isn't that much different and I suppose it could be put in a coffee grinder if it were too coarse for mixing evenly. The cost sure is better..