i have had good>great experiences in the past with charlie's two part arch crown on a 200lb pot.

while it takes some muscle, the ability to manual lift the crown of yourself is nice, one piece at a time usually, unless i am feeling really good that day......

over a few years the two halves receded from each other only a little bit and that space was easily stuffed with frax.

a pot change was always a little work but it was simple, direct, effective and done alone.

i think charlie makes great equipment and is a great guy........my 2 cents worth