Refractories

Hi Temp
2250 North Clark
Fenton MO 63026
Phone 636-677-2200
FAX 636-677-2235
Tom

Home of Morcocast refractories. Tom sells all sorts of stuff and specializes in buying out end runs when large furnaces are being built. His soft brick prices can't be beat on IFB26 and 28's. My favorite thing he sells is Morcocast 95, a 95% alumina castable made up fresh locally in very small quantities. It runs about 65 cents a lb which also makes it very inexpensive. I am about to try the Morocast 99 and will report back.