In the mid 80's Therese LaHai was at CR Loo and wanted to try and figure out the in-compatability problem. She had the base glasses and colors tested and published the COE numbers in the catalog as a rough guide. I don't remember any talk of viscosity. I think at the supplier level before this it was caveat emptor, the numbers used were the ones from the manufacturers or the E & T theoretical.