Thread: Color questions
View Single Post
  #3  
Old 10-26-2017, 07:27 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,117
Pete VanderLaan is on a distinguished road
Kugler opaques virtually all have Linear expansion coefficients from 89 on down to 85. They are not going to really fit a glass with a 96 linear expansion coefficient. Zimmermann made some incredibly beautiful colors. The mother of pearl colors are going to cause problems. Spruce Pine made SP83 specifically to address this issue.

I just took a nice little lithium pill.
__________________
Where are we going and why am I in this basket?
Reply With Quote