From my understanding the "improved" was simply trying to drop the boric content cause it was eating everyone's crucibles. Raises hand.

The oceanside version was supposed to further drop the boric, at least in the nugget form. The flake showed to be about as caustic as the original studio.

They're not really releasing expansion numbers other than that it is still compatible with the sheet.