That seems fair. I'll be really interested in the prospectus. Mine was 1500 bucks and did about 50 melts using five base glasses. It included three testing methodologies as well as calculating expansion. Just doing the base glasses alone takes a good deal of time. Then the batch room work was yet another aspect. Just very different approaches. It was exhausting. It did include a great lunch.