But do you care about the intellectual property of those you do not so revere?

I have been looking at formulas for clear glasses quite a bit recently and reading through these archives. One thing that seems a little fishy is that your NEW batch formula was realized not long after you were brought on board to help bring Cristalica to the states.

Look at the Cristalica tech notes...Barium, lots of Potassium, No lithium...a little Borax, but nothing a little extra nitrate could not resolve. Sound familiar?

Suddenly barium has started to sneak into your posts as a real positive whereas before it was a real crucible issue requiring great skill to melt (see any Glasma posts from Pete).

Were you not "inspired" by the clarity of Glasma and Cristalica? The timing just seems a little odd.