I've made a lot of "door pulls" which were basically marbles. I'd set up a large mass of glass, then spend sometimes four hours or more pulling one ball after another off of the hump. I'd usually get about 40 pulls off of a setup, which made them super heavy at the outset, but at least it got easier the longer I stayed with it.
I'd occasionally save the setups so I could pick them up later without having to fire up the main pot furnace. Still have a lot of those around. Not selling as many door pulls these days