True, it does flatten faster, but all of the cutoffs need to be taken to full charge temp to fine out. The at gather temp charge was what I saw as the main advantage of the A grade nuggets and bird droppings. It was slow, but tanks stayed fresher longer, and I wasn't beating the hell out of my furnace.

I'm in line for the Parriot, and can buy volume, so I hope to stay ahead of the supply curve. As long as it's cleaner with the off gassing than the original cristallica I should be happy.