I've done quite a few of the rare earth melts and 3% is usually my sweet spot. I mix in heavier potassium base as well. I adjust a little with Soda but I generally don't case it in clear either. Neo seems to make the glass work shorter. Its really designing around the thickness of the glass is where the color shines IMO.