Originally Posted by Josh Bernbaum View Post
It did fit my clear pretty well, was able to saw a clean ring today but expansion of this Neo melt might be a tad high because I felt just an ooch of overlap on the score in the ring. But it did saw cleanly.. Here are two pics I'm attaching of a cup in different light, all color in this (no clear case). This is just under the 4% Neo in my modified version of the Brossphate. It's about a 2.7% P2O5 content. One of my mods was adding potassium, so about 30/70 potash/soda ash in there. And a bit extra from the KNO3 I used this time. I've got some more in the pot and gonna try some thicker things tomorrow.

Thats Gorgeous!