It just gets me to whining again. When we added soda ash to the plate, finally it didn't break but that doesn't really mean a lot. I just didn't know much then. My concern now, particularly as I look to the Corning collection is glass that represents over 3000 years of process. Most stuff didn't make it but this did and it was simply because it was made without tons of stress and a lot of care. . If those old guys knew to travel to northern turkey from the Euphrates valley to find antimony, can't we do better?