In my experience 316 pits less and holds up better over time. It has also been my experience when only ordering a few sticks they will be bent unless you specify they need to be protected or secured to a piece of dunnage. It will most likely be 20 sticks. Stop collars from the usual suspects at McMaster and heater hose for grips.

That said step down punties are worth the effort. Your wrists will thank you.