[ I use SP87 for a clear when I am working it with colored glasses. I would not use it as a stand alone clear and would make either the formula Dave has listed that I wrote almost thirty years back, or a very nice 11% lead glass I pull out for special occasions. The glass should be appropriate to the project.

Just remember, get a good scale, a very good scale. I have two and I cross check every time. [/b][/quote]



Thank's Pete, Food for thought. I like the lead crystal myself. I know some of these guys probably have never had the pleasure of working a good lead glass. I'm in the process of aquiring about a ton of cullet from my employer. "They give it away". Do you believe it? I'll use it for those special projects that come up occasionaly.