I know my furnace was already falling apart, but both doors are totally cooked now. And everything seemed to start deteriorating much faster after the switch to Cristallica 8 months ago.
-------------------------------------------------
Pete, you'd need a warehouse like OCR in Atlanta, maybe one West, too, to help with shipping, methinks. Especially if you melted your blend or had it available, I could see a lot of business coming your way. But it's definitely risky as the big players might decide to step back in for the $$$.

I have to move shops, there I might be able to do batch. Not here. And I also do mobile gigs, so cullet is preferred. I know I'm in the minority.

It would be nice to have a product free from all the issues you bitch about.

Last edited by Max Epstein; 02-01-2018 at 12:48 PM.