It is no harder to melt than any other batch. It is just batch and maybe the inexperienced should stick with cullet? I don't really agree but that's ok. Get a decent respirator and a hepa filter vacuum and use both a lot.
And I don't have experience with anything other than gas furnaces.

Last edited by Sam Stang; 02-04-2018 at 03:34 PM.