My matrix on it would be

If the oceanside is like
Original System 96 Studio - OK but to short and too much borax and all the yellow crap.

New System 96 Studio - Would be fine with this longer that the original system 96 but not too long for production.

Premium nuggets - No way the original premium had lots of problems.

Premium 2.0 - Could live with it, nice and long for one offs a bit long for production.