Electrodag is the name of a product group, not a specific product.

I was hoping to find a product someone actually uses.

When I studied glassblowing in the early 1980's, we used a copper based product from a hobby shop. It was not expensive and worked really well. Later, the shop couldnt get the product anymore for some reason.

I then tried a product from Acheson, who makes electrodag. It was silver based and quite expensive, and also didnt work. It peeled off in the copper bath I was using which was quite acidic.

At that point, I moved on, and havent done electroplating on glass since.

Any suggestions are appreciated.