The guys at Hi-Temp Refractories in MO. supplied me with their Morocast 60 HS (60% alumina) product as a substitute for Mizzou to replace the 3-4" of floor that had gone to mush from pot leaks over the last 12 years. The old floor was unstable at melting temps but hard as rock at room temp. Had to use a rented electric jack hammer to get the old stuff out.

But I have listened to Pete & others long enough to decide to go Moly for the sake of lower fuel bills among other things. Just my maxon blower running 24/7 consumes $100.0 plus a month in electric charges. Now it'll only run while I'm blowing (glory).