My pleasure.

One other "playing field" observation. Phosphates will be a slightly different E&T number than the usual number that works for a particular furnace for other glasses. Not so far off it wouldn't fit, given fairly liberal guidelines for a match...or at least it's that way it is here, which, of course, may not be an issue in someone elses equipment/location.

Rollin has been melting these for a little while so he may have some observations too.