Pete VanderLaan is on a distinguished road
If it's the same sunspot studios I'm aware of, I would not have much confidence in that. At one point I had to ask the owner having trouble with my copper ruby formula

"So, What color is your black Tin?"

"white."
Just an idiot. He bought playground sand.

Actually making a well engineered clear cullet and marketing it is not an easy trick. As I look back over the last 30 years, every single one has failed either on an engineering basis or financially. with the exception of Bullseye.
The only stuff that consistently continues to be made reliably for the blowing studio is Spruce Pine Batch.