It struck me as really dangerous but he did have the thought of grounding the bench and that seemed like it could cause a lot of arcing on the rails. It is something which has my fire chief radar way out thinking about splatter. Perhaps a piece that has copper reduction on the surface? I'd be pretty sure it would trash some consumables and it is my plasma cutter but I told him I would ask.
Right now, he's weathering wood with Ammonium Chloride and then hitting it with a bench torch for the weathering effects which are quite cool.