I ran an Watlow 8CLS for 20 years... Yes Some times it can be more problematic coming down if your annealer cools slower than the time set for the segment. The next segment won't start until you reach the set point called for in that segment, even though the time set had.
Thatís why I have a fiber blanket walled annealer. It drops at just the right rate and I can control cooldowns 100%.