Hey Pete, thanks for the quick reply as always.

I'm open to suggestions here. This would be a recipe we have never made in the past so I assume there will be some trial and error with the batch.

Price really isnt a problem as long as we get chemicals that achieve the desired color and dont cause issues with compatibility.

We are looking at making a collection of alexandrite glass for our 2021 line and are starting to gather ideas and samples.

Any chance you happen to have a formula for neodymium/alexandrite glass to save me some trial and error?
It would be for an ~1000lb pot