View Single Post
  #22  
Old 04-16-2015, 05:16 AM
Dave Bross Dave Bross is offline
Registered User
 
Join Date: Apr 2002
Location: Archer FL(near Gainesville)
Posts: 2,949
Dave Bross is on a distinguished road
If you're batching your own you can make batch that goes down like a charm in a wire melter. The magic word is Lithium, and SP has quite a large percentage of it in there.

Cullet is like all your other pleasurable vices...so easy...feels so good...until.....
__________________
Art is not a thing...it's a way.