Pringle,
You just seem to have the plagues of JOB when it comes to getting bubbles out of things. I had never heard of any bad batch issue with BOMMA but I did find Charlie Parriot in what I would call less than a forthcoming mood whenever I've talked to him about it. Does the cullet have bubbles in it to begin with?

I don't know why it is so seemingly difficult. SP87 made a fine cullet as far as it goes but had the failure of the furnace as an issue. There are commercial furnaces out of South Korea that will handily melt a ton a day without issues for about 50K. The work appears to be ladling it out to turn into the cullet. Now, after two years it seems like the problem has not resolved. You still can't make money on it given the current pricing and that's dangerous.
__________________
Where are we going and why am I in this basket?
Reply With Quote