Pringle, that is so strange. I will check my bag dates this week. They are from 2019, I think from Oct 19. I did have some seed challenges when we first loaded the pot from cold. Will filled it cold and then brought it up slow, then topped it up. Doing it again I wouldn't load as much at first. would load slower in small layers. We used to load once a week but now we do it a little most nights just keeping it at our working temp of 2150 (with a side thermocouple). After the first load they eventually worked out but it just doesn't respond to a squeeze the same as the cristalica or Spectrum Sys 96.