Indeed. The code book says clearly : "Or acceptable to the authority having jurisdiction". That means common sense can prevail.

They never use it. I had one client in Georgia where the inspector decided that a moly should go in an explosion proof hood. He pulled that out of his ass.

They should have sued that SOB.