Just like running ladles for Steve Edwards, pouring 20 LARGE ladles in a day tears you upů. Steve learned that the hard way and moved to a tipping furnace near the end of his days at Alfred. Then all he had to do was push buttons for winches to pull out molds on carts from annealers and pouring was hooked up the same way. That saved costs and body parts, you don't need 4 or 5 helpers to pour your molds. This Subject of saving your body is one that is often not taken seriously enough in the glass world. Something as simple as working out to maintain the muscles you need helps significantly, as does stretching before you work. In my mind though, a well thought out and tested plan trumps everything.