David Hopman David Hopman is offline
Registered User
 
Join Date: Mar 2009
Location: Sutter Creek, CA
Posts: 440
David Hopman is on a distinguished road
I've been running the East Bay Electric batch in my Electroglass furnace for about 6 years now. It is lithium based but at a higher percentage than SP87.