Quote:
Originally Posted by Franklin Sankar View Post
Thanks for the replies. I will just have to practice much more. I blow and build up the pressure in the pipe but my seal seem to be weak so the air leaks out.
Blow hose works so good why more people donít use it?

Franklin
I use a hose all the time but never to start a bubble. Reason being that I put my starter bubble in when the glass is far too cold to put one in with a hose. The result is that I get perfect starter bubbles that are straight.