I don't consider it to be a debate unless it's a debate over whether you can afford a Porsche as opposed to a Ford Taurus.
The Taurus will get you there while the Porsche will get you there effortlessly. The Taurus may break down on the freeway on ramp, and while repairable will cause you to curse at the time. Remember those Moly elements cost more, but they have no known life span unless you break it yourself.