Go read Dan Schwoerer's paper on viscosity. I'm not apologizing for referring to Eutectics.

Keep in mind that in opals, crystals grow and they collapse and they grow again. Each time, a little less and it changes the viscosity as they change. They also change expansions understandably.

When Chuck and I were designing the glasses, we were targeting where things were the first time, not five times down the road. Down that path lies madness. . What you are doing is not something we were marketing towards. I would suggest that you set aside specific parts of that, and try making some pieces with more, and some with less sodium. See what happens. Follow the glass.