Having had an afternoon with baseball on the couch something really did occur to me which is at 4% you may begin to run into a saturation issue. 4% added means something else is diminished. I don't know what your clear base would be but that implies that it's being reduced from either the modifiers, the stabilizers or the network former. You still need a balanced glass. Lead would help you "Pack" the neo in there but it needs to be balanced overall. I have to do that with the dense black or it just is too much.