Unless your mold was a very low temp alloy, or had a contamination, it really should have done nothing in a 900* kiln. A good foundry melt should be pretty consistent throughout the entire product.

You are correct in that the oxide layer melts considerably higher, about 3200*, but the naturally occurring oxide layer is not going to be thick enough to support a hollowed out core under any kind of stress.