this may be a stupid question, but, has anyone actually seen the production setup that Spectrum has for producing this cullet? There may be flaws in the equipment and production. When I was at Spectrum many years ago, they didn't have the facilities to produce this in their factory in Woodinsville.
SP has had production problems due to equipment/production failures and this may be the same case.