Richard has certainly attested to the ease of melting my goop in a wire melter. Jim doesn't pelletize and that makes the melt even easier. It's still not a production item but he'll mix it.
To do a fluorine opal base, it needs a different formulation to match but I have it. I have not discussed mixing that with jim. It would be most unhappy in a wire melter, or rather the melter would be unhappy with it. Fluorine dictates a gas unit or a monkey pot which is a bit involved. Right now, there's no demand for either.