After spending several years under a helmet a short explanation of rod numbers... the first 2 digits are the tensile strength of the the weld left behind, ie 6011 is 60,000psi and so forth. The next number is the position. 1 is for all positions and 2 is for horixontal only..and the forth nuber has someting to do with the flux on the rod...if you want to keep your rods fresh keep them in a warm, dry environment, like an old frig(with a light bulb on inside) or maybe in the corner of an annealer. You could take them out the day b/4 you need them and they won't have soaked up all that humidity!