Originally posted by Mike Crowley
i have a 80 lb pot on ely's 13 gage kantholl 10 inch's of insulation.
i melt eltromelt, cook for 8 hours at 2280 squeeze for 4 hours , no bubs or cords just nice glass. so far the 13 gage are on there 6th week the 14 gage i was using only lasted 3 weeks .

mike
how long do you get on a set of elements? what yield do you get (lbs batch vs. lbs glass)?