It's best if you frit some clear and add the chemicals to a damp frit.

Use the Spanish iron. The only thing I want out of it is a valence switcher and any ferrous iron will do.

If you increase anything, make it the silver nitrate. Go slow it's powerful stuff.

No one ever has black tin. Do not confuse it with white tin. they arenot the same. If necessary, use tin chloride, like the fuming agent. It will reduce to tin oxide in its lower form.


You don't need classes to make color. ( It does help though) Buy glassnotes 4.0 Henry had me rewrite the batch section.