control settings

Ron , get into the output register (up down arrows together, display change, up arrow to otpt, set.

Make the register look like this,

otpt
set

ht
out1

4-20
prc1

al2n
out2

10
hys2

de1
al2

nla
lat2

off
sil2

al4n
out4

pr1
al4

10
hys4

nla
lat4

off
sil4

Then hit the display key, hit mode to enter the pid register, go past al2 and al4 settings to al4 hi and enter a value in celcius that is about 2200f.