Franklin I have used a shallow sided pan to clean fit that has been contaminated. Put some frit in the pan with the water swish the water around to get the smaller dust particles in suspension then pour the water off but not pouring off frit, this is how small time prospectors panned for gold. Put the dirt in the pan swish it around and the heavier material settles to the bottom.

i adopted a stray brittany spaniel that made a sleeping place in a wooden box that had maybe 10 kilos of white fit breaking open every bag and contaminating it with clay like mud. She was an expensive dog. Prior to that she had made a bed in two 24 by 36 by 6 inch pieces of fiberfrax even though I did not discover that until later.

Hope this helps.