If you could get the bricks cut so that there were five, I'd do the korundal/ All the brick joints in nine inch straights will kill you. Otherwise if you don't want money in it, invest a pot and run it into the ground. It's really too small to be an effective tank and you know why it isn't freestanding already. Vision is an AZS with clay binder holding the AZS chunks together and you won't like it. Not for contact. Minteq will likely be out of the price range. Try to build so the pot can be removed without destroying the rest o the tooling.