So, I am incorrect but with a large caveat. Volf indicates that Cerium can indeed be used as a decolorizer but only in the complete absence of Antimony, Arsenic or Vanadium. Even then, it is best coupled with Selenium and neodymium with a potential sneeze of manganese. It's on Pages 401-402 of Chemical Approach to Glass. It certainly surprised me and I would be inclined to stick to Erbium if I was doing it at all.